Salts for electrolytic degreasing.
It strongly degreases any metallic surface, leaving it ready to apply any galvanic bath or subsequent patina.
It is an essential process before applying any type of bath or chemical treatment.
Characteristics:
Voltage: from 4 to 6 V
stainless steel anode
Working time: between 30 and 60 seconds
Can be used with any metal
Working temperature: ambient
Preparation:
Mix 50 grams per liter of distilled water, reserving half a liter of the total you want to prepare.
Shake vigorously until you notice an increase in temperature in the preparation.
Introduce into the working tank and add another half liter of distilled water.
It strongly degreases any metallic surface, leaving it ready to apply any galvanic bath or subsequent patina.
It is an essential process before applying any type of bath or chemical treatment.
Characteristics:
Voltage: from 4 to 6 V
stainless steel anode
Working time: between 30 and 60 seconds
Can be used with any metal
Working temperature: ambient
Preparation:
Mix 50 grams per liter of distilled water, reserving half a liter of the total you want to prepare.
Shake vigorously until you notice an increase in temperature in the preparation.
Introduce into the working tank and add another half liter of distilled water.