Bright platinum bath at a concentration of 2 grams of platinum per litre. This electrolyte deposits a platinum layer with a purity of 99.97%.
It stands out for its easy application and high performance.
It belongs to the platinum group and as such has the same surface hardness as rhodium.
These characteristics make this platinum electrolyte ideal for decorative applications in the jewelry industry.
Especially suitable as an alternative to palladium plating, when used as a pre-metallization, or as a final finish on gold and silver parts in place of rhodium.
To prepare the 1 liter rhodium solution containing 2 grams per liter, you must add 920 ml of distilled water.
Characteristics:
Voltage: 3.5V
Working temperature: 60º C
Minimum exposure time: 60 seconds
Platinum titanium anode
80 ml
Instructions
1 - Do not touch the piece with your hands.
2 - Wash the parts with an ultrasonic machine.
3 - Rinse with plenty of running water.
4 - Connect the cathodic clamp of the machine to the end that holds the part.
5 - Apply the corresponding voltage
6 - Degrease 30 to 45 seconds
7 - Rinse with plenty of running water.
8 - Rinse with distilled water
9 - Wash with acidified water (Composition: 950 ml of distilled water 50 ml of chemically pure sulfuric acid).
Optional
Wash with distilled water
Soak in the platinum bath for 60 seconds
Rinse with distilled water
Dry with the usual means
Important note: It is necessary to have different containers for each step in order to avoid possible contamination by trawls.
It stands out for its easy application and high performance.
It belongs to the platinum group and as such has the same surface hardness as rhodium.
These characteristics make this platinum electrolyte ideal for decorative applications in the jewelry industry.
Especially suitable as an alternative to palladium plating, when used as a pre-metallization, or as a final finish on gold and silver parts in place of rhodium.
To prepare the 1 liter rhodium solution containing 2 grams per liter, you must add 920 ml of distilled water.
Characteristics:
Voltage: 3.5V
Working temperature: 60º C
Minimum exposure time: 60 seconds
Platinum titanium anode
80 ml
Instructions
1 - Do not touch the piece with your hands.
2 - Wash the parts with an ultrasonic machine.
3 - Rinse with plenty of running water.
4 - Connect the cathodic clamp of the machine to the end that holds the part.
5 - Apply the corresponding voltage
6 - Degrease 30 to 45 seconds
7 - Rinse with plenty of running water.
8 - Rinse with distilled water
9 - Wash with acidified water (Composition: 950 ml of distilled water 50 ml of chemically pure sulfuric acid).
Optional
Wash with distilled water
Soak in the platinum bath for 60 seconds
Rinse with distilled water
Dry with the usual means
Important note: It is necessary to have different containers for each step in order to avoid possible contamination by trawls.